General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | |||
Dureza Brinell | 241 [-] Show Material materials with Dureza Brinell of 241 [-] | Predicted Value, Transverse | |||
Elongación | 19.1 % Show Material materials with Elongación of 19.1 % | Predicted Value, Transverse | |||
19.5 % Show Material materials with Elongación of 19.5 % | Predicted Value, A80 | ||||
19.9 % Show Material materials with Elongación of 19.9 % | Predicted Value, A80 Transverse | ||||
23 % Show Material materials with Elongación of 23 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A200 | |
24.9 % Show Material materials with Elongación of 24.9 % | Predicted Value | ||||
27 % Show Material materials with Elongación of 27 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | A50 | |
Estricción | 42.7 % Show Material materials with Estricción of 42.7 % | Predicted Value | |||
43.0 % Show Material materials with Estricción of 43.0 % | Predicted Value, Transverse | ||||
Límite elástico | 205 MPa Show Material materials with Límite elástico of 205 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | RP02 |
261.6 MPa Show Material materials with Límite elástico of 261.6 MPa | Predicted Value, RP05 | ||||
271.2 MPa Show Material materials with Límite elástico of 271.2 MPa | Predicted Value, RP1 | ||||
318.8 MPa Show Material materials with Límite elástico of 318.8 MPa | Predicted Value, RP1 Transverse | ||||
358.9 MPa Show Material materials with Límite elástico of 358.9 MPa | Predicted Value, Transverse | ||||
393.8 MPa Show Material materials with Límite elástico of 393.8 MPa | Predicted Value, RP02 Transverse | ||||
405.5 MPa Show Material materials with Límite elástico of 405.5 MPa | Predicted Value, RP002 | ||||
Módulo de cizallamiento | 79.4 GPa Show Material materials with Módulo de cizallamiento of 79.4 GPa | Predicted Value | |||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | |||
Resistencia a la tracción | 380 - 515 MPa Show Material materials with Resistencia a la tracción of 380 - 515 MPa | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate | |
Resistencia al cizallamiento | 504.6 MPa Show Material materials with Resistencia al cizallamiento of 504.6 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 457.4 J/(kg·K) Show Material materials with Calor específico of 457.4 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.83 1/K Show Material materials with Coeficiente de dilatación térmica of 11.83 1/K | Predicted Value |
Conductividad térmica | 40.08 W/(m·K) Show Material materials with Conductividad térmica of 40.08 W/(m·K) | Predicted Value |
Temperatura máx. de funcionamiento | 309.6 °C Show Material materials with Temperatura máx. de funcionamiento of 309.6 °C | Predicted Value, Long |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Manganeso | 0.6 - 0.9 % Show Material materials with Manganeso of 0.6 - 0.9 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | As-Rolled or Normalized and/or Stress Relieved | ASTM A516 | Plate |
Technological properties