General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 15.1 % Show Material materials with Elongación of 15.1 % | Predicted Value, A200 | ||||
15.2 % Show Material materials with Elongación of 15.2 % | Predicted Value, A80 | |||||
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, Transverse | |||||
20.5 % Show Material materials with Elongación of 20.5 % | Predicted Value, A5 | |||||
20.7 % Show Material materials with Elongación of 20.7 % | Predicted Value, A80 Transverse | |||||
23.9 % Show Material materials with Elongación of 23.9 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Elongación of 17 % | thermomechanically rolled | EN 10225 | Sheet | ||
Estricción | 39.8 % Show Material materials with Estricción of 39.8 % | Predicted Value | ||||
44.4 % Show Material materials with Estricción of 44.4 % | Predicted Value, Transverse | |||||
Límite elástico | 263.4 MPa Show Material materials with Límite elástico of 263.4 MPa | Predicted Value, RP1 | ||||
318.6 MPa Show Material materials with Límite elástico of 318.6 MPa | Predicted Value, RP1 Transverse | |||||
425.5 MPa Show Material materials with Límite elástico of 425.5 MPa | Predicted Value, RP02 | |||||
431.2 MPa Show Material materials with Límite elástico of 431.2 MPa | Predicted Value, Transverse | |||||
487.7 MPa Show Material materials with Límite elástico of 487.7 MPa | Predicted Value, RP02 Transverse | |||||
500.1 MPa Show Material materials with Límite elástico of 500.1 MPa | Predicted Value, RP05 | |||||
528 MPa Show Material materials with Límite elástico of 528 MPa | Predicted Value, RP002 | |||||
20 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 405 MPa Show Material materials with Límite elástico of 405 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 415 MPa Show Material materials with Límite elástico of 415 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 420 MPa Show Material materials with Límite elástico of 420 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 440 MPa Show Material materials with Límite elástico of 440 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 460 MPa Show Material materials with Límite elástico of 460 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Módulo de cizallamiento | 79.9 GPa Show Material materials with Módulo de cizallamiento of 79.9 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 500 - 700 MPa Show Material materials with Resistencia a la tracción of 500 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | |
20 °C | 500 - 690 MPa Show Material materials with Resistencia a la tracción of 500 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 680 MPa Show Material materials with Resistencia a la tracción of 500 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 675 MPa Show Material materials with Resistencia a la tracción of 500 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 665 MPa Show Material materials with Resistencia a la tracción of 500 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 660 MPa Show Material materials with Resistencia a la tracción of 500 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 700 MPa Show Material materials with Resistencia a la tracción of 505 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 690 MPa Show Material materials with Resistencia a la tracción of 505 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 680 MPa Show Material materials with Resistencia a la tracción of 505 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 675 MPa Show Material materials with Resistencia a la tracción of 505 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 665 MPa Show Material materials with Resistencia a la tracción of 505 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 505 - 660 MPa Show Material materials with Resistencia a la tracción of 505 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 700 MPa Show Material materials with Resistencia a la tracción of 515 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 690 MPa Show Material materials with Resistencia a la tracción of 515 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 680 MPa Show Material materials with Resistencia a la tracción of 515 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 675 MPa Show Material materials with Resistencia a la tracción of 515 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 665 MPa Show Material materials with Resistencia a la tracción of 515 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 515 - 660 MPa Show Material materials with Resistencia a la tracción of 515 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 700 MPa Show Material materials with Resistencia a la tracción of 520 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 690 MPa Show Material materials with Resistencia a la tracción of 520 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 680 MPa Show Material materials with Resistencia a la tracción of 520 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 675 MPa Show Material materials with Resistencia a la tracción of 520 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 665 MPa Show Material materials with Resistencia a la tracción of 520 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 520 - 660 MPa Show Material materials with Resistencia a la tracción of 520 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 700 MPa Show Material materials with Resistencia a la tracción of 530 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 690 MPa Show Material materials with Resistencia a la tracción of 530 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 680 MPa Show Material materials with Resistencia a la tracción of 530 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 675 MPa Show Material materials with Resistencia a la tracción of 530 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 665 MPa Show Material materials with Resistencia a la tracción of 530 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 530 - 660 MPa Show Material materials with Resistencia a la tracción of 530 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 700 MPa Show Material materials with Resistencia a la tracción of 540 - 700 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 690 MPa Show Material materials with Resistencia a la tracción of 540 - 690 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 680 MPa Show Material materials with Resistencia a la tracción of 540 - 680 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 675 MPa Show Material materials with Resistencia a la tracción of 540 - 675 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 665 MPa Show Material materials with Resistencia a la tracción of 540 - 665 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 540 - 660 MPa Show Material materials with Resistencia a la tracción of 540 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Resistencia al cizallamiento | 544.9 MPa Show Material materials with Resistencia al cizallamiento of 544.9 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 453.1 J/(kg·K) Show Material materials with Calor específico of 453.1 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.89 1/K Show Material materials with Coeficiente de dilatación térmica of 11.89 1/K | Predicted Value |
Conductividad térmica | 37.03 W/(m·K) Show Material materials with Conductividad térmica of 37.03 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 - 0.055 % Show Material materials with Aluminio of 0.015 - 0.055 % | thermomechanically rolled | EN 10225 | Sheet |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % | thermomechanically rolled | EN 10225 | Sheet |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Boro | 0.001 % Show Material materials with Boro of 0.001 % | thermomechanically rolled | EN 10225 | Sheet |
Calcio | 0.005 % Show Material materials with Calcio of 0.005 % | thermomechanically rolled | EN 10225 | Sheet |
Carbono | 0.14 % Show Material materials with Carbono of 0.14 % | thermomechanically rolled | EN 10225 | Sheet |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | thermomechanically rolled | EN 10225 | Sheet |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Manganeso | 1.65 % Show Material materials with Manganeso of 1.65 % | thermomechanically rolled | EN 10225 | Sheet |
Molibdeno | 0.25 % Show Material materials with Molibdeno of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Niobio | 0.04 % Show Material materials with Niobio of 0.04 % | thermomechanically rolled | EN 10225 | Sheet |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Níquel | 0.7 % Show Material materials with Níquel of 0.7 % | thermomechanically rolled | EN 10225 | Sheet |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Silicona | 0.15 - 0.55 % Show Material materials with Silicona of 0.15 - 0.55 % | thermomechanically rolled | EN 10225 | Sheet |
Titanio | 0.025 % Show Material materials with Titanio of 0.025 % | thermomechanically rolled | EN 10225 | Sheet |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % | thermomechanically rolled | EN 10225 | Sheet |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |