General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 2.7 % Show Supplier Material materials with Absorción de agua of 2.7 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-2/1A | 5mm/min | |
Módulo de flexión | 9.5 GPa Show Supplier Material materials with Módulo de flexión of 9.5 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 11.6 GPa Show Supplier Material materials with Módulo elástico of 11.6 GPa | dry | ISO 527-2/1A | 1mm/min | |
Resistencia a la flexión | 245 MPa Show Supplier Material materials with Resistencia a la flexión of 245 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-2/1A | 5mm/min | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de fusión | 217 °C Show Supplier Material materials with Temperatura de fusión of 217 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 10000 Ω/sq Show Supplier Material materials with Surface resistivity of 10000 Ω/sq | 50%RH | IEC 60093 | 500V |
100000 Ω/sq Show Supplier Material materials with Surface resistivity of 100000 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 100 Ω·cm Show Supplier Material materials with Volume resistivity of 100 Ω·cm | 50%RH | IEC 60093 | 500V |
1000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Eletrically Dissipative, Increased Electrical Conductivity, Anti-Static Modified, Heat Stabilized | |
Fillers | 15% Carbon Fiber | |
Processing methods | Injection Molding |