General
Property | Temperature | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|---|
Absorción de agua | 5.5 % Show Supplier Material materials with Absorción de agua of 5.5 % | 2 mm | ISO 62 | immersion at 23°C | ||
Densidad | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | ISO 1183 | dry | |||
Moisture absorption | 23 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | 2 mm | ISO 62 | 50%RH |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-2/1A | 5mm/min | |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 6.9 GPa Show Supplier Material materials with Módulo de flexión of 6.9 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 5.2 GPa Show Supplier Material materials with Módulo elástico of 5.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
7.9 GPa Show Supplier Material materials with Módulo elástico of 7.9 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 185 MPa Show Supplier Material materials with Resistencia a la flexión of 185 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU | |
23 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | 50%RH | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Thickness | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
7e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-05 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | IEC 60695-2-12 | 1 mm, 2 mm | ||||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 1 mm | ||||
750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 2 mm | |||||
Temperatura de flexión bajo carga | 230 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 230 °C | ISO 75/2Af | 1.80 MPa | ||||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Temperatura de reblandecimiento Vicat | 240 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 240 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 | Thickness tested (mm): 1.5, Class: 5VA, Standard: UL 94 | Thickness tested (mm): 1.5, Class: 5VA, Standard: IEC 60695-11-20 at dry condition (Burning behaviour) | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V | |
Índice de seguimiento comparativo | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | dry | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Black | |
Features | Flame Retardant, Halogen-free, Heat Stabilized | |
Fillers | 25% Glass Fiber | |
Processing methods | Injection Molding |