General
Property | Value | Thickness | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Absorción de agua | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | 2 mm | ISO 62 | 24h immersion at 23°C | |
Densidad | 1.52 g/cm³ Show Supplier Material materials with Densidad of 1.52 g/cm³ | ISO 1183 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | 50%RH | ISO 527-2/1A | 5mm/min | |
2.1 % Show Supplier Material materials with Elongación of 2.1 % | dry | ISO 527-2/1A | 5mm/min | ||
Módulo de flexión | 14.2 GPa Show Supplier Material materials with Módulo de flexión of 14.2 GPa | dry | ISO 178 | 2mm/min | |
Módulo elástico | 15.5 GPa Show Supplier Material materials with Módulo elástico of 15.5 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
15.8 GPa Show Supplier Material materials with Módulo elástico of 15.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Resistencia a la flexión | 370 MPa Show Supplier Material materials with Resistencia a la flexión of 370 MPa | dry | ISO 178 | 2mm/min | |
Resistencia a la tracción | 240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
245 MPa Show Supplier Material materials with Resistencia a la tracción of 245 MPa | dry | ISO 527-2/1A | 5mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | 50%RH | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 293 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 293 °C | ISO 75/2Af | 1.80 MPa | ||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | ISO 11357-1/-3 | 10°C/min | ||
Inflamabilidad | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | 330/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Contracción of 0.7 % | 330/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE, Food Contact | |
Color | Natural | |
Fillers | 40% Glass Fiber | |
Processing methods | Injection Molding |