General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 205 - 800 mm Show Supplier Material materials with Ancho of 205 - 800 mm | |
Diámetro | 20 - 800 mm Show Supplier Material materials with Diámetro of 20 - 800 mm | |
Espesor | 800 mm Show Supplier Material materials with Espesor of 800 mm | max. |
Longitud | 2000 - 5800 mm Show Supplier Material materials with Longitud of 2000 - 5800 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Steels |
Dureza Brinell | 23.0 °C | 269 [-] Show Supplier Material materials with Dureza Brinell of 269 [-] | |
Elongación | 23.0 °C | 12 % Show Supplier Material materials with Elongación of 12 % | |
Límite elástico | 23.0 °C | 835 MPa Show Supplier Material materials with Límite elástico of 835 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | Typical for Steels |
Resistencia a la tracción | 23.0 °C | 980 MPa Show Supplier Material materials with Resistencia a la tracción of 980 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 23.0 °C | 44.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 44.5 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 2.48E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.48E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % |
Carbono | 0.38 - 0.43 % Show Supplier Material materials with Carbono of 0.38 - 0.43 % |
Cromo | 0.7 - 0.9 % Show Supplier Material materials with Cromo of 0.7 - 0.9 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 0.6 - 0.8 % Show Supplier Material materials with Manganeso of 0.6 - 0.8 % |
Molibdeno | 0.2 - 0.3 % Show Supplier Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 1.65 - 2 % Show Supplier Material materials with Níquel of 1.65 - 2 % |
Silicona | 0.15 - 0.35 % Show Supplier Material materials with Silicona of 0.15 - 0.35 % |