DIN 17663 Grade 2.0720

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Copper

45 - 49 %

Show Material materials with Copper of 45 - 49 %

Iron

0.5 %

Show Material materials with Iron of 0.5 %

Lead

0.1 %

Show Material materials with Lead of 0.1 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Other

Rest Zn, total 0.1