DIN 1733-1 Grade 2.0877

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.7 g/cm³

Show Material materials with Density of 8.7 g/cm³

Thermal

PropertyTemperatureValue

Melting point

1100 - 1145 °C

Show Material materials with Melting point of 1100 - 1145 °C

Thermal conductivity

23.0 °C

45 W/(m·K)

Show Material materials with Thermal conductivity of 45 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

4.00E+6 - 5.00E+6 S/m

Show Material materials with Electrical conductivity of 4.00E+6 - 5.00E+6 S/m

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Iron

2.5 %

Show Material materials with Iron of 2.5 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.5 - 2 %

Show Material materials with Manganese of 0.5 - 2 %

Nickel

9 - 11 %

Show Material materials with Nickel of 9 - 11 %

Other

Rest Cu, total 0.5

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

0.5 %

Show Material materials with Titanium of 0.5 %