Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze | ||
Tensile strength | 252 MPa Show Material materials with Tensile strength of 252 MPa | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.005 % Show Material materials with Aluminium of 0.005 % | ASTM B30, ASTM B505 | Casting |
Antimony | 0.2 % Show Material materials with Antimony of 0.2 % | ASTM B30 | |
0.25 % Show Material materials with Antimony of 0.25 % | ASTM B505 | Casting | |
Copper | 86 - 89 % Show Material materials with Copper of 86 - 89 % | ASTM B30, ASTM B505 | Casting |
Iron | 0.15 % Show Material materials with Iron of 0.15 % | ASTM B30 | |
0.15 % Show Material materials with Iron of 0.15 % | ASTM B30 | ||
0.2 % Show Material materials with Iron of 0.2 % | ASTM B505 | Casting | |
0.2 % Show Material materials with Iron of 0.2 % | |||
Lead | 1 - 2.3 % Show Material materials with Lead of 1 - 2.3 % | ASTM B30 | |
1 - 2.5 % Show Material materials with Lead of 1 - 2.5 % | ASTM B505 | Casting | |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Nickel of 1 % | ASTM B505 | Casting | |
Phosphorus | 0.25 % Show Material materials with Phosphorus of 0.25 % | ASTM B30 | |
0.3 % Show Material materials with Phosphorus of 0.3 % | ASTM B30 | ||
1.5 % Show Material materials with Phosphorus of 1.5 % | ASTM B505 | Casting | |
Silicon | 0.005 % Show Material materials with Silicon of 0.005 % | ASTM B30, ASTM B505 | Casting |
Sulfur | 0.05 % Show Material materials with Sulfur of 0.05 % | ASTM B30, ASTM B505 | Casting |
Tin | 9 - 11 % Show Material materials with Tin of 9 - 11 % | ASTM B505 | Casting |
9.3 - 11 % Show Material materials with Tin of 9.3 - 11 % | ASTM B30 | ||
Zinc | 0.7 % Show Material materials with Zinc of 0.7 % | ASTM B505 | Casting |
0.8 % Show Material materials with Zinc of 0.8 % | ASTM B30 |