Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminium | 10.5 - 11.5 % Show Material materials with Aluminium of 10.5 - 11.5 % | ASTM B30, ASTM B271, ASTM B505 |
Chromium | 0.05 % Show Material materials with Chromium of 0.05 % | ASTM B30 |
Cobalt | 0.2 % Show Material materials with Cobalt of 0.2 % | ASTM B30 |
Copper | 74.5 % Show Material materials with Copper of 74.5 % | ASTM B30, ASTM B271, ASTM B505 |
Iron | 4 - 5.5 % Show Material materials with Iron of 4 - 5.5 % | ASTM B30, ASTM B271, ASTM B505 |
Lead | 0.03 % Show Material materials with Lead of 0.03 % | ASTM B30, ASTM B271, ASTM B505 |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % | ASTM B30 |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % | ASTM B30, ASTM B271, ASTM B505 |
Nickel | 4.2 - 6 % Show Material materials with Nickel of 4.2 - 6 % | ASTM B30, ASTM B271, ASTM B505 |
Silicon | 0.15 % Show Material materials with Silicon of 0.15 % | ASTM B30, ASTM B271, ASTM B505 |
Tin | 0.25 % Show Material materials with Tin of 0.25 % | ASTM B30, ASTM B271, ASTM B505 |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | ASTM B30, ASTM B271, ASTM B505 |