Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

120 - 156 GPa

Show Material materials with Elastic modulus of 120 - 156 GPa

Typical for Cast Copper Nickel Grade

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Cast Copper Nickel Grade

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Typical for Cast Copper Nickel Grade

Melting point

1100 - 1240 °C

Show Material materials with Melting point of 1100 - 1240 °C

Typical for Cast Copper Nickel Grade

Specific heat capacity

23.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Typical for Cast Copper Nickel Grade

Thermal conductivity

23.0 °C

23 - 45 W/(m·K)

Show Material materials with Thermal conductivity of 23 - 45 W/(m·K)

Typical for Cast Copper Nickel Grade

Chemical properties

PropertyValue

Bismuth

2E-3 %

Show Material materials with Bismuth of 2E-3 %

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Cobalt

0.05 %

Show Material materials with Cobalt of 0.05 %

Iron

1 - 1.4 %

Show Material materials with Iron of 1 - 1.4 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Manganese

1 - 1.4 %

Show Material materials with Manganese of 1 - 1.4 %

Nickel

28 - 32 %

Show Material materials with Nickel of 28 - 32 %

Other

Rest Cu, total 0.30

Phosphorus

5E-3 %

Show Material materials with Phosphorus of 5E-3 %

Silicon

0.2 - 0.4 %

Show Material materials with Silicon of 0.2 - 0.4 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %