CEN/TS 13388 Grade CC484K

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Antimony

0.1 %

Show Material materials with Antimony of 0.1 %

Copper

84.5 - 87.5 %

Show Material materials with Copper of 84.5 - 87.5 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.3 %

Show Material materials with Lead of 0.3 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

1.5 - 2.5 %

Show Material materials with Nickel of 1.5 - 2.5 %

Phosphorus

0.05 - 0.4 %

Show Material materials with Phosphorus of 0.05 - 0.4 %

Silicon

0.01 %

Show Material materials with Silicon of 0.01 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %

Tin

11 - 13 %

Show Material materials with Tin of 11 - 13 %

Zinc

0.4 %

Show Material materials with Zinc of 0.4 %