BS 1400 Grade CC495K

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

96 - 120 GPa

Show Material materials with Elastic modulus of 96 - 120 GPa

Typical for Cast Copper Bronze

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Cast Copper Bronze

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K

Typical for Cast Copper Bronze

Melting point

760 - 1060 °C

Show Material materials with Melting point of 760 - 1060 °C

Typical for Cast Copper Bronze

Specific heat capacity

23.0 °C

376 - 440 J/(kg·K)

Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K)

Typical for Cast Copper Bronze

Thermal conductivity

23.0 °C

12 - 81 W/(m·K)

Show Material materials with Thermal conductivity of 12 - 81 W/(m·K)

Typical for Cast Copper Bronze

Chemical properties

PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Antimony

0.5 %

Show Material materials with Antimony of 0.5 %

Iron

0.15 %

Show Material materials with Iron of 0.15 %

Lead

8.5 - 11 %

Show Material materials with Lead of 8.5 - 11 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

2 %

Show Material materials with Nickel of 2 %

Other

Rest Cu, total 0.50

Phosphorus

0.1 %

Show Material materials with Phosphorus of 0.1 %

Silicon

0.02 %

Show Material materials with Silicon of 0.02 %

Sulfur

0.1 %

Show Material materials with Sulfur of 0.1 %

Tin

9 - 11 %

Show Material materials with Tin of 9 - 11 %

Zinc

1 %

Show Material materials with Zinc of 1 %