CEN/TS 13388 Grade CF125C

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Boron

0.02 - 0.05 %

Show Material materials with Boron of 0.02 - 0.05 %

Nickel

2.5 - 3.5 %

Show Material materials with Nickel of 2.5 - 3.5 %

Other

Rest Cu, total 0.15. excluded Ag