Chemical properties

PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

0.03 %

Show Material materials with Cadmium of 0.03 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Other

Rest Cu, Zn+Cd < 0.05, Alle Total 0.25

Phosphorus

5.7 - 6.3 %

Show Material materials with Phosphorus of 5.7 - 6.3 %

Silver

4.5 - 5.5 %

Show Material materials with Silver of 4.5 - 5.5 %

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %