Chemical properties

PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Copper

46 - 50 %

Show Material materials with Copper of 46 - 50 %

Iron

0.25 %

Show Material materials with Iron of 0.25 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

8 - 11 %

Show Material materials with Nickel of 8 - 11 %

Other

Rest Zn, total 0.2

Silicon

0.15 - 0.4 %

Show Material materials with Silicon of 0.15 - 0.4 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %