Properties

Chemical properties

PropertyValue

Aluminium

5E-3 %

Show Material materials with Aluminium of 5E-3 %

Cadmium

0.03 %

Show Material materials with Cadmium of 0.03 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Other

Rest Cu, each 0.1, total 0.4

Phosphorus

0.01 - 0.4 %

Show Material materials with Phosphorus of 0.01 - 0.4 %

Tin

11 - 13 %

Show Material materials with Tin of 11 - 13 %

Zinc

0.05 %