CEN/TS 13388 Grade CF735R

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

13 - 17 %

Show Material materials with Cadmium of 13 - 17 %

Copper

39 - 41 %

Show Material materials with Copper of 39 - 41 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

total 0.15

Phosphorus

8E-3 %

Show Material materials with Phosphorus of 8E-3 %

Silicon

0.05 %

Show Material materials with Silicon of 0.05 %

Silver

19 - 21 %

Show Material materials with Silver of 19 - 21 %

Zinc

23 - 27 %

Show Material materials with Zinc of 23 - 27 %