Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

15.5 - 19.5 %

Show Material materials with Cadmium of 15.5 - 19.5 %

Copper

29 - 31 %

Show Material materials with Copper of 29 - 31 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

total 0.15

Phosphorus

8E-3 %

Show Material materials with Phosphorus of 8E-3 %

Silicon

0.05 %

Show Material materials with Silicon of 0.05 %

Silver

24 - 26 %

Show Material materials with Silver of 24 - 26 %

Zinc

25.5 - 29.5 %

Show Material materials with Zinc of 25.5 - 29.5 %