CEN/TS 13388 Grade CF739R

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

0.03 %

Show Material materials with Cadmium of 0.03 %

Copper

35 - 37 %

Show Material materials with Copper of 35 - 37 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

total 0.15

Phosphorus

8E-3 %

Show Material materials with Phosphorus of 8E-3 %

Silicon

0.05 %

Show Material materials with Silicon of 0.05 %

Silver

29 - 31 %

Show Material materials with Silver of 29 - 31 %

Tin

1.5 - 2.5 %

Show Material materials with Tin of 1.5 - 2.5 %

Zinc

30 - 34 %

Show Material materials with Zinc of 30 - 34 %