Chemical properties

PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Bismuth

0.03 %

Show Material materials with Bismuth of 0.03 %

Cadmium

0.03 %

Show Material materials with Cadmium of 0.03 %

Copper

43 - 45 %

Show Material materials with Copper of 43 - 45 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

total 0.15

Phosphorus

8E-3 %

Show Material materials with Phosphorus of 8E-3 %

Silicon

0.05 - 0.25 %

Show Material materials with Silicon of 0.05 - 0.25 %

Silver

19 - 21 %

Show Material materials with Silver of 19 - 21 %

Zinc

34 - 38 %

Show Material materials with Zinc of 34 - 38 %