EN 1981 Grade CM123C

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Lithium

1.6 - 2.2 %

Show Material materials with Lithium of 1.6 - 2.2 %

Other

Rest Cu, each 0.03, total 0.2

Selenium

2E-4 %

Show Material materials with Selenium of 2E-4 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %