EN 1978 Grade CR001A

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Typical for Wrought Copper Pure / Low Alloyed Copper

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

95 - 98 GPa

Show Material materials with Elastic modulus of 95 - 98 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Wrought Copper Pure / Low Alloyed Copper

Shear modulus

23.0 °C

48 GPa

Show Material materials with Shear modulus of 48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper Pure / Low Alloyed Copper

Melting point

965 - 1100 °C

Show Material materials with Melting point of 965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Specific heat capacity

23.0 °C

377 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 377 - 420 J/(kg·K)

Typical for Wrought Copper Pure / Low Alloyed Copper

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.86E+7 S/m

Show Material materials with Electrical conductivity of 5.86E+7 S/m

Electrical resistivity

23.0 °C

1.71E-8 Ω·m

Show Material materials with Electrical resistivity of 1.71E-8 Ω·m

Chemical properties

PropertyValue

Antimony

4E-4 %

Show Material materials with Antimony of 4E-4 %

Arsenic

5E-4 %

Show Material materials with Arsenic of 5E-4 %

Bismuth

2E-4 %

Show Material materials with Bismuth of 2E-4 %

Iron

1E-3 %

Show Material materials with Iron of 1E-3 %

Lead

5E-4 %

Show Material materials with Lead of 5E-4 %

Other

Rest Cu, Total 0.0065, (As+Cd+Cr+Mn+P+Sb) < 0.0015 %, (Bi+Se+Te) < 0.0003 %, of which (Se+Te) < 0.00030 %, (Co+Fe+Ni+Si+Sn+Zn) < 0.0020 %

Silver

2.5E-3 %

Show Material materials with Silver of 2.5E-3 %

Sulfur

1.5E-3 %

Show Material materials with Sulfur of 1.5E-3 %

Tellurium

2E-4 %

Show Material materials with Tellurium of 2E-4 %