Chemical properties

PropertyValue

Bismuth

5E-4 %

Show Material materials with Bismuth of 5E-4 %

Copper

99.95 %

Show Material materials with Copper of 99.95 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Other

total 0.03. excluded Ag, P

Phosphorus

1E-3 - 6E-3 %

Show Material materials with Phosphorus of 1E-3 - 6E-3 %