EN 12861 Grade CS052B

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Arsenic

5E-3 %

Show Material materials with Arsenic of 5E-3 %

Copper

99.5 %

Show Material materials with Copper of 99.5 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.1 %

Show Material materials with Lead of 0.1 %

Nickel

0.02 %

Show Material materials with Nickel of 0.02 %

Other

Cu: including Ag to max. 0.015% and O to 0.06%, each 0.002

Phosphorus

0.06 %

Show Material materials with Phosphorus of 0.06 %

Tin

0.06 %

Show Material materials with Tin of 0.06 %

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %