PN/H 87026 Grade CuSn10P

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Wrought Copper High Copper Alloy

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper High Copper Alloy

Melting point

855 - 1090 °C

Show Material materials with Melting point of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Antimony

0.25 %

Show Material materials with Antimony of 0.25 %

Arsenic

0.1 %

Show Material materials with Arsenic of 0.1 %

Bismuth

0.01 %

Show Material materials with Bismuth of 0.01 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.2 %

Show Material materials with Lead of 0.2 %

Magnesium

0.02 %

Show Material materials with Magnesium of 0.02 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

0.5 %

Show Material materials with Nickel of 0.5 %

Other

Rest Cu, total 0.8

Phosphorus

0.5 - 1 %

Show Material materials with Phosphorus of 0.5 - 1 %

Silicon

0.02 %

Show Material materials with Silicon of 0.02 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %

Tin

9 - 11 %

Show Material materials with Tin of 9 - 11 %

Zinc

0.3 %

Show Material materials with Zinc of 0.3 %