CEN/TS 13388 Grade CW006A R200, H040

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

42 %

Show Material materials with Elongation of 42 %

Hardness, Vickers

20.0 °C

40 - 65 [-]

Show Material materials with Hardness, Vickers of 40 - 65 [-]

Tensile strength

20.0 °C

200 - 250 MPa

Show Material materials with Tensile strength of 200 - 250 MPa

Yield strength Rp0.2

20.0 °C

100 MPa

Show Material materials with Yield strength Rp0.2 of 100 MPa

Chemical properties

PropertyValue

Copper

99.9 %

Show Material materials with Copper of 99.9 %

Other

total 0.05. excluded Ag, Ni, O

Oxygen

0.1 %

Show Material materials with Oxygen of 0.1 %

Selenium

2E-4 %

Show Material materials with Selenium of 2E-4 %