PropertyValue

Dimensions

Durchmesser

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

5 %

Show Material materials with Elongation of 5 %

Elongation A100

20.0 °C

3 %

Show Material materials with Elongation A100 of 3 %

Hardness, Brinell

20.0 °C

100 [-]

Show Material materials with Hardness, Brinell of 100 [-]

Hardness, Vickers

20.0 °C

110 [-]

Show Material materials with Hardness, Vickers of 110 [-]

Tensile strength

20.0 °C

350 MPa

Show Material materials with Tensile strength of 350 MPa

Yield strength Rp0.2

20.0 °C

330 MPa

Show Material materials with Yield strength Rp0.2 of 330 MPa

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

5.86E+7 S/m

Show Material materials with Electrical conductivity of 5.86E+7 S/m

Electrical resistivity

20.0 °C

1.71E-8 Ω·m

Show Material materials with Electrical resistivity of 1.71E-8 Ω·m

Chemical properties

PropertyValue

Antimony

4E-4 %

Show Material materials with Antimony of 4E-4 %

Arsenic

5E-4 %

Show Material materials with Arsenic of 5E-4 %

Bismuth

2E-4 %

Show Material materials with Bismuth of 2E-4 %

Iron

1E-3 %

Show Material materials with Iron of 1E-3 %

Lead

5E-4 %

Show Material materials with Lead of 5E-4 %

Other

total 0.0065

Silver

2.5E-3 %

Show Material materials with Silver of 2.5E-3 %

Sulfur

1.5E-3 %

Show Material materials with Sulfur of 1.5E-3 %

Tellurium

2E-4 %

Show Material materials with Tellurium of 2E-4 %