BS 6017 Grade CW019A

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Bismuth

1E-3 %

Show Material materials with Bismuth of 1E-3 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Other

total 0.03, Cu+Ag > 99.95

Silver

0.09 %