General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

20 %

Show Material materials with Elongation of 20 %

Elongation A50

20.0 °C

20 %

Show Material materials with Elongation A50 of 20 %

Hardness, Vickers

20.0 °C

60 - 130 [-]

Show Material materials with Hardness, Vickers of 60 - 130 [-]

Tensile strength

20.0 °C

240 MPa

Show Material materials with Tensile strength of 240 MPa

Yield strength Rp0.2

20.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

2.50E+7 S/m

Show Material materials with Electrical conductivity of 2.50E+7 S/m

Electrical resistivity

20.0 °C

4E-8 Ω·m

Show Material materials with Electrical resistivity of 4E-8 Ω·m

Chemical properties

PropertyValue

Beryllium

0.4 - 0.7 %

Show Material materials with Beryllium of 0.4 - 0.7 %

Cobalt

0.8 - 1.3 %

Show Material materials with Cobalt of 0.8 - 1.3 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Nickel

0.8 - 1.3 %

Show Material materials with Nickel of 0.8 - 1.3 %

Other

Rest Cu, total 0.5