See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Durchmesser

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

105 GPa

Show Material materials with Elastic modulus of 105 GPa

Elongation

20.0 °C

50 %

Show Material materials with Elongation of 50 %

Elongation A100

20.0 °C

40 %

Show Material materials with Elongation A100 of 40 %

Hardness, Brinell

20.0 °C

85 - 115 [-]

Show Material materials with Hardness, Brinell of 85 - 115 [-]

Hardness, Vickers

20.0 °C

90 - 120 [-]

Show Material materials with Hardness, Vickers of 90 - 120 [-]

Tensile strength

20.0 °C

380 MPa

Show Material materials with Tensile strength of 380 MPa

Yield strength Rp0.2

20.0 °C

260 MPa

Show Material materials with Yield strength Rp0.2 of 260 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

100.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Melting point

970 - 1025 °C

Show Material materials with Melting point of 970 - 1025 °C

Thermal conductivity

20.0 °C

38 W/(m·K)

Show Material materials with Thermal conductivity of 38 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

3.80E+6 - 4.00E+6 S/m

Show Material materials with Electrical conductivity of 3.80E+6 - 4.00E+6 S/m

Electrical resistivity

20.0 °C

2.5E-7 - 2.63E-7 Ω·m

Show Material materials with Electrical resistivity of 2.5E-7 - 2.63E-7 Ω·m

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

0.7 - 1.3 %

Show Material materials with Manganese of 0.7 - 1.3 %

Other

Rest Cu, total 0.5

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

2.7 - 3.2 %

Show Material materials with Silicon of 2.7 - 3.2 %

Zinc

0.4 %