Chemical properties

PropertyValue

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Arsenic

2E-3 %

Show Material materials with Arsenic of 2E-3 %

Bismuth

1E-3 %

Show Material materials with Bismuth of 1E-3 %

Cadmium

0.25 - 0.4 %

Show Material materials with Cadmium of 0.25 - 0.4 %

Iron

5E-3 %

Show Material materials with Iron of 5E-3 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Nickel

2E-3 %

Show Material materials with Nickel of 2E-3 %

Other

Rest Cu, total 0.30

Sulfur

5E-3 %

Show Material materials with Sulfur of 5E-3 %

Tin

2E-3 %

Show Material materials with Tin of 2E-3 %

Zinc

5E-3 %