General

PropertyTemperatureValue

Density

20.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Dimension

PropertyValue

Dimensions

Durchmesser

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

5 %

Show Material materials with Elongation of 5 %

Hardness, Brinell

20.0 °C

170 [-]

Show Material materials with Hardness, Brinell of 170 [-]

Hardness, Vickers

20.0 °C

180 [-]

Show Material materials with Hardness, Vickers of 180 [-]

Tensile strength

20.0 °C

650 MPa

Show Material materials with Tensile strength of 650 MPa

Yield strength Rp0.2

20.0 °C

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa

Chemical properties

PropertyValue

Copper

42 - 45 %

Show Material materials with Copper of 42 - 45 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

1 - 2.5 %

Show Material materials with Lead of 1 - 2.5 %

Manganese

4.5 - 6 %

Show Material materials with Manganese of 4.5 - 6 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Other

Rest Zn, total 0.2

Tin

0.2 %

Show Material materials with Tin of 0.2 %