CEN/TS 13388 Grade CW460K R460, H130

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Wanddicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Brinell

20.0 °C

125 - 160 [-]

Show Material materials with Hardness, Brinell of 125 - 160 [-]

Hardness, Vickers

20.0 °C

130 - 165 [-]

Show Material materials with Hardness, Vickers of 130 - 165 [-]

Tensile strength

20.0 °C

460 MPa

Show Material materials with Tensile strength of 460 MPa

Yield strength Rp0.2

20.0 °C

280 MPa

Show Material materials with Yield strength Rp0.2 of 280 MPa

Chemical properties

PropertyValue

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.1 - 0.5 %

Show Material materials with Lead of 0.1 - 0.5 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Cu, total 0.2

Phosphorus

0.2 - 0.4 %

Show Material materials with Phosphorus of 0.2 - 0.4 %

Tin

7.5 - 9 %

Show Material materials with Tin of 7.5 - 9 %

Zinc

0.3 %

Show Material materials with Zinc of 0.3 %