CEN/TS 13388 Grade CW500L R230, H045

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

45 %

Show Material materials with Elongation of 45 %

Elongation A50

20.0 °C

36 %

Show Material materials with Elongation A50 of 36 %

Hardness, Vickers

20.0 °C

45 - 75 [-]

Show Material materials with Hardness, Vickers of 45 - 75 [-]

Tensile strength

20.0 °C

230 - 280 MPa

Show Material materials with Tensile strength of 230 - 280 MPa

Yield strength Rp0.2

20.0 °C

130 MPa

Show Material materials with Yield strength Rp0.2 of 130 MPa

Thermal

PropertyValue

Melting point

1050 - 1065 °C

Show Material materials with Melting point of 1050 - 1065 °C

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Copper

94 - 96 %

Show Material materials with Copper of 94 - 96 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.1

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Technological properties

Property
Brazing

hard brazing : very good, soft brazing: very good

Workability

Cold forming degree between anneals: max. 90 %, general (condition): very good