CEN/TS 13388 Grade CW603N R360

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.5 g/cm³

Show Material materials with Density of 8.5 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

102 GPa

Show Material materials with Elastic modulus of 102 GPa

Elongation

23.0 °C

20 %

Show Material materials with Elongation of 20 %

Hardness, Brinell

23.0 °C

90 [-]

Show Material materials with Hardness, Brinell of 90 [-]

Hardness, Vickers

23.0 °C

90 [-]

Show Material materials with Hardness, Vickers of 90 [-]

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Tensile strength

23.0 °C

360 MPa

Show Material materials with Tensile strength of 360 MPa

Yield strength Rp0.2

23.0 °C

180 MPa

Show Material materials with Yield strength Rp0.2 of 180 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

2.06E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.06E-5 1/K

100.0 °C

2.06E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.06E-5 1/K

Melting point

885 - 900 °C

Show Material materials with Melting point of 885 - 900 °C

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

23.0 °C

100 W/(m·K)

Show Material materials with Thermal conductivity of 100 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

1.47E+7 S/m

Show Material materials with Electrical conductivity of 1.47E+7 S/m

Electrical resistivity

23.0 °C

6.8E-8 Ω·m

Show Material materials with Electrical resistivity of 6.8E-8 Ω·m

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

60 - 62 %

Show Material materials with Copper of 60 - 62 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

2.5 - 3.5 %

Show Material materials with Lead of 2.5 - 3.5 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.2

Tin

0.2 %