PropertyValue

Aluminium

5E-3 %

Show Material materials with Aluminium of 5E-3 %

Antimony

0.5 %

Show Material materials with Antimony of 0.5 %

Copper

70 - 76 %

Show Material materials with Copper of 70 - 76 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

16 - 22 %

Show Material materials with Lead of 16 - 22 %

Nickel

1 %

Show Material materials with Nickel of 1 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

5E-3 %

Show Material materials with Silicon of 5E-3 %

Tin

6 - 9 %

Show Material materials with Tin of 6 - 9 %

Zinc

1 %

Show Material materials with Zinc of 1 %