GOST 859 Grade M0 k

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Antimony

1E-3 %

Show Material materials with Antimony of 1E-3 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

5E-4 %

Show Material materials with Bismuth of 5E-4 %

Iron

1E-3 %

Show Material materials with Iron of 1E-3 %

Lead

2E-3 %

Show Material materials with Lead of 2E-3 %

Nickel

1E-3 %

Show Material materials with Nickel of 1E-3 %

Other

Cu+Ag > 99.97

Oxygen

0.02 %

Show Material materials with Oxygen of 0.02 %

Phosphorus

1E-3 %

Show Material materials with Phosphorus of 1E-3 %

Silver

2E-3 %

Show Material materials with Silver of 2E-3 %

Sulfur

2E-3 %

Show Material materials with Sulfur of 2E-3 %

Tin

1E-3 %

Show Material materials with Tin of 1E-3 %

Zinc

1E-3 %

Show Material materials with Zinc of 1E-3 %