Chemical properties

PropertyValue

Antimony

0.05 %

Show Material materials with Antimony of 0.05 %

Arsenic

0.01 %

Show Material materials with Arsenic of 0.01 %

Bismuth

3E-3 %

Show Material materials with Bismuth of 3E-3 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Other

Cu+Ag > 99.50

Oxygen

0.08 %

Show Material materials with Oxygen of 0.08 %

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

Tin

0.05 %