Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

100 - 125 GPa

Show Material materials with Elastic modulus of 100 - 125 GPa

Typical for Wrought Copper Brass

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K

Typical for Wrought Copper Brass

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

23.0 °C

100 - 234 W/(m·K)

Show Material materials with Thermal conductivity of 100 - 234 W/(m·K)

Typical for Wrought Copper Brass

Chemical properties

PropertyValue

Aluminium

2E-3 %

Show Material materials with Aluminium of 2E-3 %

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Arsenic

2E-3 %

Show Material materials with Arsenic of 2E-3 %

Bismuth

2E-3 %

Show Material materials with Bismuth of 2E-3 %

Copper

74 - 77 %

Show Material materials with Copper of 74 - 77 %

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Other

Rest Zn, total 0.3

Phosphorus

0.01 %

Show Material materials with Phosphorus of 0.01 %

Silicon

0.45 - 0.75 %

Show Material materials with Silicon of 0.45 - 0.75 %

Sulfur

2E-3 %

Show Material materials with Sulfur of 2E-3 %

Tin

2E-3 %

Show Material materials with Tin of 2E-3 %