PN/H 87053 Grade MN

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Arsenic

2E-3 %

Show Material materials with Arsenic of 2E-3 %

Bismuth

2E-3 %

Show Material materials with Bismuth of 2E-3 %

Carbon

2E-3 %

Show Material materials with Carbon of 2E-3 %

Iron

5E-3 %

Show Material materials with Iron of 5E-3 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Nickel

0.52 - 0.58 %

Show Material materials with Nickel of 0.52 - 0.58 %

Other

Rest Cu, total 0.10

Phosphorus

2E-3 %

Show Material materials with Phosphorus of 2E-3 %

Silicon

2E-3 %

Show Material materials with Silicon of 2E-3 %

Sulfur

5E-3 %

Show Material materials with Sulfur of 5E-3 %