GOST 492 Grade MNMc3-12

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Arsenic

5E-3 %

Show Material materials with Arsenic of 5E-3 %

Bismuth

2E-3 %

Show Material materials with Bismuth of 2E-3 %

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Iron

0.5 %

Show Material materials with Iron of 0.5 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Magnesium

0.03 %

Show Material materials with Magnesium of 0.03 %

Manganese

11.5 - 13.5 %

Show Material materials with Manganese of 11.5 - 13.5 %

Nickel

2.5 - 3.5 %

Show Material materials with Nickel of 2.5 - 3.5 %

Other

Rest Cu, total 0.90

Phosphorus

5E-3 %

Show Material materials with Phosphorus of 5E-3 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %