GB 5233 Grade QBe1.9-0.1

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.15 %

Show Material materials with Aluminium of 0.15 %

Beryllium

1.85 - 2.1 %

Show Material materials with Beryllium of 1.85 - 2.1 %

Iron

0.15 %

Show Material materials with Iron of 0.15 %

Lead

5E-3 %

Show Material materials with Lead of 5E-3 %

Magnesium

0.07 - 0.13 %

Show Material materials with Magnesium of 0.07 - 0.13 %

Nickel

0.2 - 0.4 %

Show Material materials with Nickel of 0.2 - 0.4 %

Other

Rest Cu, total 0.5

Silicon

0.15 %

Show Material materials with Silicon of 0.15 %

Titanium

0.1 - 0.25 %

Show Material materials with Titanium of 0.1 - 0.25 %