Alliance NdFeB N-40UH

Want to keep this datasheet? Save it now in your required format

Description

Neodymium Magnets, also known as NdFeB or simply Neo, are the strongest and most commonly used magnet materials for high tech motors and sensors

This material data has been provided by Alliance LLC.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.5 g/cm³

Show Supplier Material materials with Density of 7.5 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

150 - 160 GPa

Show Supplier Material materials with Elastic modulus of 150 - 160 GPa

Flexural strength

23.0 °C

180 - 270 MPa

Show Supplier Material materials with Flexural strength of 180 - 270 MPa

Tensile strength

23.0 °C

80 MPa

Show Supplier Material materials with Tensile strength of 80 MPa

Thermal

PropertyValue

Max service temperature

180 °C

Show Supplier Material materials with Max service temperature of 180 °C

Magnetic

PropertyTemperatureValueComment

Coercive force

23.0 °C

938000 A/m

Show Supplier Material materials with Coercive force of 938000 A/m

min

Intrinsic coercivity

23.0 °C

1.99E+6 A/m

Show Supplier Material materials with Intrinsic coercivity of 1.99E+6 A/m

min

Maximum energy product

23.0 °C

302 - 334 kJ/m³

Show Supplier Material materials with Maximum energy product of 302 - 334 kJ/m³

Remanence

23.0 °C

1.26 - 1.32 T

Show Supplier Material materials with Remanence of 1.26 - 1.32 T

Reversible temperature coefficient coercivity

23.0 °C

0.55 %/ °C

Show Supplier Material materials with Reversible temperature coefficient coercivity of 0.55 %/ °C

Reversible temperature coefficient remanence

23.0 °C

0.1 %/ °C

Show Supplier Material materials with Reversible temperature coefficient remanence of 0.1 %/ °C