Alliance Alnico 5

Want to keep this datasheet? Save it now in your required format

Description

Alnico magnets can be Cast or Sintered. High Br and resistance to extreme temperatures

This material data has been provided by Alliance LLC.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.3 g/cm³

Show Supplier Material materials with Density of 7.3 g/cm³

Thermal

PropertyValue

Max service temperature

550 °C

Show Supplier Material materials with Max service temperature of 550 °C

Magnetic

PropertyTemperatureValue

Coercive force

23.0 °C

51000 A/m

Show Supplier Material materials with Coercive force of 51000 A/m

Intrinsic coercivity

23.0 °C

51000 A/m

Show Supplier Material materials with Intrinsic coercivity of 51000 A/m

Maximum energy product

23.0 °C

40 kJ/m³

Show Supplier Material materials with Maximum energy product of 40 kJ/m³

Remanence

23.0 °C

1.25 T

Show Supplier Material materials with Remanence of 1.25 T

Reversible temperature coefficient coercivity

23.0 °C

0.03 %/ °C

Show Supplier Material materials with Reversible temperature coefficient coercivity of 0.03 %/ °C

Reversible temperature coefficient remanence

23.0 °C

0.02 %/ °C

Show Supplier Material materials with Reversible temperature coefficient remanence of 0.02 %/ °C

Technological properties

Property
Application areas

Holding, Instruments

Other

Cast magnet material, great for holding devices