1070A H16 Non-Heat Treatable Al Wrought Alloy

Want to keep this datasheet? Save it now in your required format

Description

Excellent surface finishing properties (bright, anodizing ...) and corrosion resistance.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.69 g/cm³

Show Supplier Material materials with Density of 2.69 g/cm³

Dimension

PropertyValue

Thickness

0.2 - 3 mm

Show Supplier Material materials with Thickness of 0.2 - 3 mm

Mechanical

PropertyTemperatureValueComment

Bending angle 180°

23.0 °C

1 °/t

Show Supplier Material materials with Bending angle 180° of 1 °/t

according to EN 485-2

Bending angle 90°

23.0 °C

1 °/t

Show Supplier Material materials with Bending angle 90° of 1 °/t

according to EN 485-2

Elastic modulus

23.0 °C

70 GPa

Show Supplier Material materials with Elastic modulus of 70 GPa

Elongation A50

23.0 °C

2 %

Show Supplier Material materials with Elongation A50 of 2 %

according to EN 485-2

Hardness, HBW

23.0 °C

26 - 36 [-]

Show Supplier Material materials with Hardness, HBW of 26 - 36 [-]

according to EN 485-2

Shear modulus

23.0 °C

26.5 GPa

Show Supplier Material materials with Shear modulus of 26.5 GPa

Tensile strength

23.0 °C

80 - 150 MPa

Show Supplier Material materials with Tensile strength of 80 - 150 MPa

according to EN 485-2

Yield strength

23.0 °C

55 - 90 MPa

Show Supplier Material materials with Yield strength of 55 - 90 MPa

according to EN 485-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

20-100°C

Thermal conductivity

23.0 °C

138 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 138 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

4.9E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.9E-8 Ω·m

Chemical properties

PropertyValueComment

Copper

0.03 %

Show Supplier Material materials with Copper of 0.03 %

Iron

0.25 %

Show Supplier Material materials with Iron of 0.25 %

Magnesium

0.03 %

Show Supplier Material materials with Magnesium of 0.03 %

Manganese

0.03 %

Show Supplier Material materials with Manganese of 0.03 %

Other

0.03 %

Show Supplier Material materials with Other of 0.03 %

Min.

Silicon

0.2 %

Show Supplier Material materials with Silicon of 0.2 %

Titanium

0.03 %

Show Supplier Material materials with Titanium of 0.03 %

Zinc

0.07 %

Show Supplier Material materials with Zinc of 0.07 %

Technological properties

Property
Anodizing

Excellent

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges

Corrosion properties

Excellent

Welding

Excellent

Workability

Excellent