1090 Non-Heat Treatable Al Wrought Alloy

Alternative and trade names
1090, Al99.75Cu
.XLSX
.PDF
Save

Description

Excellent surface finishing properties (bright, anodizing ...)

Related Standards

Properties

General

Density ρ

2.7 g/cm³ at 20 °C

Mechanical

Elastic modulus E

70 GPa at 20 °C

Shear modulus G

26.5 GPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.3E-5 1/K at 100 °C

20-100°C

Thermal conductivity λ

235 W/(m·K) at 20 °C

Electrical

Electrical resistivity ρel

2.8E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

0.07 %

Si

0.07 %

V

0.05 %

Ga

0.03 %

Zn

0.03 %

More

Technological properties

Anodizing

Excellent

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels; Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Decoration

Corrosion properties

Excellent

Workability

Excellent

This material data has been provided by Aludium.