Universal work hardening alloy offering medium strength, very good formability, and very good corrosion resistance. Good durability properties.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.69 g/cm³

Show Supplier Material materials with Density of 2.69 g/cm³

Dimension

PropertyValue

Thickness

0.2 - 6 mm

Show Supplier Material materials with Thickness of 0.2 - 6 mm

Mechanical

PropertyTemperatureValue

Bending angle 180°

23.0 °C

2 °/t

Show Supplier Material materials with Bending angle 180° of 2 °/t

Bending angle 90°

23.0 °C

0.5 - 2.5 °/t

Show Supplier Material materials with Bending angle 90° of 0.5 - 2.5 °/t

Elastic modulus

23.0 °C

68.6 GPa

Show Supplier Material materials with Elastic modulus of 68.6 GPa

Elongation A50

23.0 °C

3 - 8 %

Show Supplier Material materials with Elongation A50 of 3 - 8 %

Hardness, HBW

23.0 °C

62 [-]

Show Supplier Material materials with Hardness, HBW of 62 [-]

Tensile strength

23.0 °C

210 - 250 MPa

Show Supplier Material materials with Tensile strength of 210 - 250 MPa

Yield strength

23.0 °C

140 MPa

Show Supplier Material materials with Yield strength of 140 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

20-100°C

Thermal conductivity

23.0 °C

153 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 153 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

4.5E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.5E-8 Ω·m

Chemical properties

PropertyValue

Chromium

0.15 %

Show Supplier Material materials with Chromium of 0.15 %

Copper

0.15 %

Show Supplier Material materials with Copper of 0.15 %

Iron

0.5 %

Show Supplier Material materials with Iron of 0.5 %

Magnesium

1.7 - 2.4 %

Show Supplier Material materials with Magnesium of 1.7 - 2.4 %

Manganese

0.1 - 0.5 %

Show Supplier Material materials with Manganese of 0.1 - 0.5 %

Other

0.05 - 0.15 %

Show Supplier Material materials with Other of 0.05 - 0.15 %

Silicon

0.4 %

Show Supplier Material materials with Silicon of 0.4 %

Titanium

0.15 %

Show Supplier Material materials with Titanium of 0.15 %

Zinc

0.15 %

Show Supplier Material materials with Zinc of 0.15 %

Technological properties

Property
Anodizing

Excellent

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Tubes: Industrial tubes, Pipes; Wind energy: Nacelle coverings, rotor hub, stairs;

Corrosion properties

Excellent

Welding

Very Good

Workability

Very Good