Description

Good for items intended to come into contact with food.

Equivalent Materials

This material data has been provided by Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.73 g/cm³

Show Supplier Material materials with Density of 2.73 g/cm³

Dimension

PropertyValue

Thickness

0.08 - 0.2 mm

Show Supplier Material materials with Thickness of 0.08 - 0.2 mm

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

15 %

Show Supplier Material materials with Elongation A50 of 15 %

Tensile strength

23.0 °C

110 - 150 MPa

Show Supplier Material materials with Tensile strength of 110 - 150 MPa

Yield strength

23.0 °C

40 - 80 MPa

Show Supplier Material materials with Yield strength of 40 - 80 MPa

Chemical properties

PropertyValue

Chromium

0.2 %

Show Supplier Material materials with Chromium of 0.2 %

Copper

0.3 %

Show Supplier Material materials with Copper of 0.3 %

Iron

0.6 - 1.2 %

Show Supplier Material materials with Iron of 0.6 - 1.2 %

Magnesium

0.2 - 0.6 %

Show Supplier Material materials with Magnesium of 0.2 - 0.6 %

Manganese

0.4 - 1 %

Show Supplier Material materials with Manganese of 0.4 - 1 %

Silicon

0.6 %

Show Supplier Material materials with Silicon of 0.6 %

Zinc

0.25 %

Show Supplier Material materials with Zinc of 0.25 %

Technological properties

Property
Application areas

Semi-rigid and corrugated: Smooth wall