Description

This product is available in the following forms: Bright round bars, Billets, Ingots

Related Standards

This material data has been provided by AMBI.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

12 %

Show Supplier Material materials with Elongation of 12 %

Tensile strength

23.0 °C

750 - 950 MPa

Show Supplier Material materials with Tensile strength of 750 - 950 MPa

Yield strength

23.0 °C

550 MPa

Show Supplier Material materials with Yield strength of 550 MPa

Chemical properties

PropertyValue

Carbon

0.33 - 0.45 %

Show Supplier Material materials with Carbon of 0.33 - 0.45 %

Chromium

15.5 - 17.5 %

Show Supplier Material materials with Chromium of 15.5 - 17.5 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

Molybdenum

0.8 - 1.3 %

Show Supplier Material materials with Molybdenum of 0.8 - 1.3 %

Nickel

1 %

Show Supplier Material materials with Nickel of 1 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Technological properties

Property
Application areas

Automobile